Powder Eutalloy 10680 500G
SKU: 10680Coatings on metals including steel, stainless steel, cast iron and nickel alloys.
Alloy nickel-based powder for anti-wear protective coatings.
$104.70 Inc. GST
- FREE shipping on all orders over $200!
| Powder Properties | |
|---|---|
| Nominal Composition: | Nickel, Boron, Silicon |
| Hall Flow Rate: | 14 seconds |
| Bulk Density: | 4.8 g/cc |
| Coating Properties | |
| Typical Tensile Shear Strength: | 75,000 psi |
| Typical Hardness: | HRB 95 |
| Maximum Service Temperature: | 1200°F (649° C) |
| Thickness Limit: | Unlimited |
General-purpose build-up and dimensional restoration for cast iron and steel parts such as:
- Gears Shafts
- Patterns
- Clutches
- Templates
Preparation:
All surfaces to be coated should be thoroughly cleaned, removing all contaminants, oxides and grease. Thin surfaces and edges require no preheating. However, large, heavy and cast iron parts of all thickness should be heated to about 575°F (approx. 302°C) (blue hot).
Coating instructions:
For coating operations the flame of the Eutalloy B or SuperJet S torch should be adjusted to neutral with the powder feed on. To prevent oxidation of the base material we recommend spraying a thin coat of Eutalloy 10224. A second coat is delivered in the following manner: preheat locally to fusion point (when the first coat becomes glazed in appearance), then spray and fuse the second coat simultaneously. Move progressively along, spraying and fusing, until the entire surface is covered. Distance between the cone of the flame and the piece should be .25 – .75 inch. Leave the part to cool slowly and away from air currents. Where possible, place it in vermiculite or cover with a thermal blanket